Mar 09, 2023 Mesaj bırakın

Notes for aluminum profile extrusion die test and aluminum extrusion process

First, in the aluminum alloy profile extrusion die test and aluminum extrusion process, we should pay attention to the following aspects:

 

A. Determine the temperature of the die bar before extrusion of aluminum alloy profiles, whether it meets the requirements of extrusion temperature, and whether the heating has penetrated core (the placement of the die in the heating furnace is very important, and there should be a certain heating gap between the die and the die). First, in the aluminum alloy profile extrusion die test and aluminum extrusion process, we should pay attention to the following aspects:

 

A. Determine the temperature of the die bar before extrusion of aluminum alloy profiles, whether it meets the requirements of extrusion temperature, and whether the heating has penetrated core (the placement of the die in the heating furnace is very important, and there should be a certain heating gap between the die and the die).

 

B. Aluminum extrusion die must be aligned to the center, so as to avoid collapse and die plug phenomenon.

 

C. Suitable extrusion speed should be selected for different aluminum alloy profile moulds, so as to avoid poor discharge caused by too fast and too urgent. D. In the process of extrusion of aluminum alloy profiles, we should pay attention to the quality of aluminum rods to avoid mold collapse caused by impurities of aluminum rods, etc.

 

Two, aluminum extrusion mold repair is a very important link, but the first thing to consider is the strength of the mold repair, to ensure the strength of aluminum extrusion mold on the basis of repair. Less than the last degree is generally not used to burn welding, because burning welding has a significant impact on the life of the die. Especially the welding of working belt, easy to shorten the life. For the quick and slow repair of profiles, generally use the slow place repair and do not use the fast place slow. So far, reducing the burden on the mold construction can ensure its life to a certain extent. Of course, improving the level of mold repair and reducing the number of mold trials is also one of the ways to improve the service life of the mold.

 

Three, in the process of mold cooking, special attention should be paid to the link of taking punching material, especially in some screw holes or more fragile places, otherwise, it is easy to destroy the mold.

 

Four. The handling process of aluminum extrusion die should be carried out carefully to avoid bumping into the work belt and other places. Before the mold is put into the warehouse, be sure to clean it and check the mold carefully and deeply to see if there are any small cracks and damage.

 

Five, for the finished production of the mold must carry out effective management of its process data, such as mold repair program, processing details, extrusion process, etc. Because these can become the subsequent supplementary mold or similar mold copy object, this can effectively improve the mold on the machine pass rate.

 

In short, the improvement of extrusion die life depends on the perfect link of design, manufacturing, use and subsequent maintenance processes. Relying on a single link can not effectively achieve the purpose, through the effective integration of all links, I believe that the life of the mold can be improved accordingly.

 

B. Aluminum extrusion die must be aligned to the center, so as to avoid collapse and die plug phenomenon.

 

C. Suitable extrusion speed should be selected for different aluminum alloy profile moulds, so as to avoid poor discharge caused by too fast and too urgent. D. In the process of extrusion of aluminum alloy profiles, we should pay attention to the quality of aluminum rods to avoid mold collapse caused by impurities of aluminum rods, etc.

 

Two, aluminum extrusion mold repair is a very important link, but the first thing to consider is the strength of the mold repair, to ensure the strength of aluminum extrusion mold on the basis of repair. Less than the last degree is generally not used to burn welding, because burning welding has a significant impact on the life of the die. Especially the welding of working belt, easy to shorten the life. For the quick and slow repair of profiles, generally use the slow place repair and do not use the fast place slow. So far, reducing the burden on the mold construction can ensure its life to a certain extent. Of course, improving the level of mold repair and reducing the number of mold trials is also one of the ways to improve the service life of the mold.

 

Three, in the process of mold cooking, special attention should be paid to the link of taking punching material, especially in some screw holes or more fragile places, otherwise, it is easy to destroy the mold.

 

Four. The handling process of aluminum extrusion die should be carried out carefully to avoid bumping into the work belt and other places. Before the mold is put into the warehouse, be sure to clean it and check the mold carefully and deeply to see if there are any small cracks and damage.

 

Five, for the finished production of the mold must carry out effective management of its process data, such as mold repair program, processing details, extrusion process, etc. Because these can become the subsequent supplementary mold or similar mold copy object, this can effectively improve the mold on the machine pass rate.

 

In short, the improvement of extrusion die life depends on the perfect link of design, manufacturing, use and subsequent maintenance processes. Relying on a single link can not effectively achieve the purpose, through the effective integration of all links, I believe that the life of the mold can be improved accordingly.

Soruşturma göndermek